What is Low Hydrogen electrodes, Their Storage & Baking Procedure?

Low Hydrogen electrodes, Their Storage & Baking Procedure? Low-hydrogen electrodes are SMAW electrodes that contain less than 0.6% coating moisture — as per ASME Section IIC, SFA 5.1- Table 10, compared to … Continue reading What is Low Hydrogen electrodes, Their Storage & Baking Procedure?