Online hardness convertor Hardness Conversion ASTM E140-97 from HV: Vickers HardnessHB: Brinell Hardness 10 mm C-ball 3000 kgfHK: Knoop Hardness 500 gf and overHRA: Rockwell A Hardness 60 kgf.HRB: Rockwell B Hardness 100 kgf.HRC: Rockwell C Hardness 150 kgf.HRD: Rockwell D Hardness 100 kgf.HR15N: Rockwell Superficial 15 kgf.HR30N: Rockwell Superficial 30 kgf.HR45N: Rockwell Superficial 45 kgf.HSc: Scleroscope Hardness to HV: Vickers HardnessHB: Brinell Hardness 10 mm C-Ball 3000 kgfHRC: Rockwell C Hardness 150 kgf. Related Posts:Online Hardness Conversion CalculatorWhat is hardness & types of Hardness tests?Carbon Steel & Low Alloy Steel Hardness Test…What is Martensite in Steel?ASTM A108 Steel Welding GuideTypes of Destructive Testing4140 vs 4130 Steel- Find the differencesInconel 625How to Weld AISI 4145