Online Hardness Conversion Calculator Hardness Conversion Calculator Home Welding Welding Calculator Hardness Conversion ASTM E140-97 from HV: Vickers Hardness HB: Brinell Hardness 10 mm C-ball 3000 kgf HK: Knoop Hardness 500 gf and over HRA: Rockwell A Hardness 60 kgf. HRB: Rockwell B Hardness 100 kgf. HRC: Rockwell C Hardness 150 kgf. HRD: Rockwell D Hardness 100 kgf. HR15N: Rockwell Superficial 15 kgf. HR30N: Rockwell Superficial 30 kgf. HR45N: Rockwell Superficial 45 kgf. HSc: Scleroscope Hardness to HV: Vickers Hardness HB: Brinell Hardness 10 mm C-Ball 3000 kgf HRC: Rockwell C Hardness 150 kgf. Related Posts:What is hardness & types of Hardness tests?Online hardness convertorCarbon Steel & Low Alloy Steel Hardness Test…How to Ball Tungsten for Aluminum Welding430 Stainless Steel vs other SteelLearn Different Welding Positions for Plate & Pipe